ROWALIT® 200-60A
Heat stabilized Copolyamide
Chemical character
Copolyamide
Melting range
110 – 120 °C DSC
Melt Flow Index
90 g / 10 Min. (MFI 160°C / 2,16 kg)
Ratio of renewable raw materials
0 %
Dry cleaning resistance
very good
Typical application
Hotmelt Lamination
Appearance
slight transparent granule
Fusing conditions with flow-through-press
Lamination temperature: 100 – 140 °C
Pneumatic pressure: 3 – 5 N/cm²
Time: 12 – 20 seconds
Application
Slot die, Coating roller (hotmelt), Foilextrusion; Rototherm