TPU
Thermoplastic Polyurethanes (TPU) are unique products with different properties that are interesting for a great variety of applications:
- High resistance against washing and cleaning methods (textile applications)
- High elasticity within complete hardnesses range
- Good resistance against oils, fats and many solvents
- Free of plasticizers
- […]
Therefore TPU finds utilization in many areas such as textile, sport- and leisure industry, military, medical or automotive.
The product series ROWALIT™ 500 usually covers a melting range of 55-145°C.
| Product Name | Download | Type | Melting range | Melt Flow Index | Powder Sizes
|
Ratio of renewable raw materials | Eco-Passport | Biodegradability | Resistance to dry cleaning | Washing resistance | Heat resistance | Fusing conditions with flow-through-press | Appearance | |||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| ROWALIT™ 500-1 | TPU | 90 – 105 °C DSC | 4 g / 10 Min. (MFI 160°C) |
|
no | 90 °C |
Fugentemperatur: 100 – 120 °C Druck: 3 – 5 N/cm² Zeit: 10 – 15 Sekunden |
White powder | ||||||||||
| ROWALIT™ 500-3 | TPU | 60 – 80 °C DSC | 80 g / 10 Min. (MFI 160°C) |
|
no | fair | 60 °C | 50 °C |
Fugentemperatur: 75 – 80 °C Druck: 2 – 4 N/cm² Zeit: 10 – 15 Sekunden |
White powder | ||||||||
| ROWALIT™ 500-50 | TPU | 6 g / 10 Min. (MFI 160°C) |
|
0 % | ✓ | no | good | 60 °C | 60 °C |
Fugentemperatur: 120 – 145 °C Druck: 2 – 4 N/cm² Zeit: 10 – 20 Sekunden |
White powder | |||||||
| ROWALIT™ 500-57 | TPU | 4 g / 10 Min. (MFI 160°C) |
|
0 % | ✓ | no | good | 60 °C | 90 °C |
Fugentemperatur: 120 – 145 °C Druck: 2 – 4 N/cm² Zeit: 10 – 20 Sekunden |
White powder | |||||||
| ROWALIT™ 500-59 | TPU | 125 – 140 °C DSC | 30 g / 10 Min. (MFI 160°C) |
|
✓ | no | good | 90 °C | 110 °C |
Fugentemperatur: 140 – 150 °C Druck: 3 – 5 N/cm² Zeit: 12 – 20 Sekunden |
White powder | |||||||
| ROWALIT™ 500-7 | TPU | 62 – 66 °C DSC | 20 g / 10 Min. (MFI 160°C) |
|
fair |
Fugentemperatur: 75 – 85 °C Druck: 2 – 4 N/cm² Zeit: 10 – 15 Sekunden |
White powder | |||||||||||
| ROWALIT™ 500-SIT-23 | TPU | 20 g / 10 Min. (MFI 160°C) |
|
✓ | no | good | 60 °C | 90 °C |
Fugentemperatur: 125 – 145 °C Druck: 2 – 4 N/cm² Zeit: 12 – 20 Sekunden |
White powder | ||||||||
| ROWALIT™ 500-SIT-37 | TPU | 115 – 125 °C DSC | 20 g / 10 Min. (MFI 160°C) |
|
0 % | ✓ | no | good | 60 °C | 90 °C |
Fugentemperatur: 120 – 145 °C Druck: 2 – 4 N/cm² Zeit: 12 – 20 Sekunden |
White powder | ||||||
| ROWALIT™ 500-SIT-38 | TPU | 20 g / 10 Min. (MFI 160°C) |
|
0 % | ✓ | no | good | 60 °C | 90 °C |
Fugentemperatur: 125 – 145 °C Druck: 2 – 4 N/cm² Zeit: 12 – 20 Sekunden |
White powder |