Thermoplastic Polyurethanes (TPU) are unique products with different properties that are interesting for a great variety of applications:
- High resistance against washing and cleaning methods (textile applications)
- High elasticity within complete hardnesses range
- Good resistance against oils, fats and many solvents
- Free of plasticizers
- […]
Therefore TPU finds utilization in many areas such as textile, sport- and leisure industry, military, medical or automotive.
The product series ROWALIT® 500 usually covers a melting range of 55-145°C.
Product name | Type | Melting range | Softening point | Melt Flow Index | Powder sizes | Resistance to dry cleaning | Hand iron | Enzyme washing | Washing resistance | Steam resistance | Stone-wash resistance | Heat resistance | Fusing conditions with flow-through-press | Appearance | ||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Pastedot | Doubledot | Powderdot | Scatter | Granules | Lamination temperature | Pneumatic pressure | Time | |||||||||||||
ROWALIT 500-1 | TPU | 90 – 105 °C DSC | 80 – 85 °C | 4 g / 10 Min. (MFI 160°C) | ✕ | ✕ | ✓ | 100 – 500 µm | ✓ | 90 °C | 100 – 120 °C | 3 – 5 N/cm² | 10 – 15 Sek. | White powder | ||||||
ROWALIT 500-3 | TPU | 60 – 80 °C DSC | 60 – 64 °C | 80 g / 10 Min. (MFI 160°C) | ✕ | ✕ | ✕ | 100 – 500 µm | ✓ | fair | yes | 60 °C | 50 °C | 75 – 80 °C | 2 – 4 N/cm² | 10 – 15 Sek. | White powder | |||
ROWALIT 500-7 | TPU | 62 – 66 °C DSC | 50 – 60 °C | 20 g / 10 Min. (MFI 160°C) | ✕ | ✕ | ✕ | 100 – 500 µm | ✓ | 75 – 85 °C | 2 – 4 N/cm² | 10 – 15 Sek. | ||||||||
ROWALIT 500-SIT-23 | TPU | 105 – 120 °C | 20 g / 10 Min. (MFI 160°C) |
0 – 63 µm 0 – 80 µm |
80 – 200 µm | ✓ | 100 – 500 µm | ✓ | good | no | 60 °C | yes | 90 °C | 125 – 145 °C | 2 – 4 N/cm² | 12 – 20 Sek. | White powder | |||
ROWALIT 500-SIT-37 | TPU | 115 – 125 °C DSC | 110 – 120 °C | 20 g / 10 Min. (MFI 160°C) |
0 – 63 µm 0 – 80 µm |
80 – 200 µm | ✕ | 100 – 500 µm | ✓ | good | 60 °C | yes | 90 °C | 120 – 145 °C | 2 – 4 N/cm² | 12 – 20 Sek. | White powder | |||
BIOPOW® 5038 | Biobased Products, TPU | 100 – 125 °C DSC | 105 – 120 °C | 20 g / 10 Min. (MFI 160°C) |
0 – 63 µm 0 – 80 µm |
80 – 200 µm | ✕ | 0 – 500 µm | ✓ | good | 60 °C | 90 °C | 125 – 145 °C | 2 – 4 N/cm² | 12 – 20 Sek. | White powder | ||||
ROWALIT 500-SIT-38 | TPU | 105 – 120 °C | 20 g / 10 Min. (MFI 160°C) |
0 – 63 µm 0 – 80 µm |
80 – 200 µm | ✕ | 100 – 500 µm | ✓ | good | no | 60 °C | yes | 90 °C | 125 – 145 °C | 2 – 4 N/cm² | 12 – 20 Sek. | White powder | |||
ROWALIT 500-50 | TPU | 85 – 105 °C | 6 g / 10 Min. (MFI 160°C) | 0 – 80 µm | 80 – 200 µm | ✓ | 100 – 500 µm | ✓ | good | yes | 60 °C | no | 60 °C | 120 – 145 °C | 2 – 4 N/cm² | 12 – 20 Sek. | White powder | |||
ROWALIT 500-57 | TPU | 100 – 120 °C | 4 g / 10 Min. (MFI 160°C) | 0 – 80 µm | 80 – 200 µm | ✓ | 100 – 500 µm | ✓ | good | no | 60 °C | no | 90 °C | 120 – 145 °C | 2 – 4 N/cm² | 12 – 20 Sek. | White powder | |||
ROWALIT 500-59 | TPU | 125 – 140 °C DSC | 120 – 130 °C | 30 g / 10 Min. (MFI 160°C) | 0 – 80 µm | 80 – 200 µm | ✕ | 100 – 500 µm | ✓ | good | no | 90 °C | very good | 110 °C | 140 – 150 °C | 3 – 5 N/cm² | 12 – 20 Sek. | White powder |