Type | Copolyamide |
Melting range / °C DSC | 100 - 120 |
Melting viscosity / g | |
MFI 160°C, 2.16 kg, 10 min. | 180 |
Chemical Basis | Copolyamide |
Powder sizes | |
Pastedot | ![]() |
Doubledot | ![]() |
Powderdot | ![]() |
Scatter | ![]() |
Granules | ![]() |
Resistance to dry cleaning | very good |
Washing resistance in °C |
60°C |
Steam resistance | good |
Heat resistance in °C |
90 |
Fusing conditions with flow-through-press | |
Lamination temperature in °C | 110 - 145 |
Pneumatic pressure N / cm² | 3 - 5 |
Time in sec. | 10 - 15 |
Appearance | White powder |
Interlinings with fusing conditions and low viscosity at good fastness profile; siliconized fabrics; in paste dot coating as crosslinkable thermoplast as base dot in doubledot process or single dot in direct lamination - outstanding fastnesses are reached
Guide recipe recommendation
|
Water / H2O | 55 kg | |
ROWAFLEX® DF 2 | 0.2 kg | |
ROWAFLEX® X 600 | 3 kg | |
ROWALIT® 200-63, 0-80 | 30 kg | |
ROWAFLEX® TH 3 | 0.4 kg | |
ROWAFLEX® X 100 | 10 kg |