The copolyester series ROWALIT® 400 is applied in the apparel industry and steadily expanding in technical items. They cover a melting range of 80-135°C.
Copolyester hotmelt adhesives offer good bond strength and wash resistance on PES and traditional blends like PES/Cotton textiles. Dry cleaning resistance is limited.
Product name | Type | Melting range | Melt Flow Index | Powder sizes | Resistance to dry cleaning | Hand iron | Enzyme washing | Washing resistance | Steam resistance | Stone-wash resistance | Heat resistance | Fusing conditions with flow-through-press | Appearance | ||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Pastedot | Doubledot | Powderdot | Scatter | Granules | Lamination temperature | Pneumatic pressure | Time | ||||||||||||
ROWALIT® BIOPOW 1036 | Biobased Products, Copolyester | 115 – 115 °C DSC | 22 g / 10 Min. (MFI 190°C) | 0 – 80 µm | 80 – 200 µm | ✓ | 100 – 500 µm | ✓ | 60 °C | 95 °C | 125 – 150 °C | 3 – 5 N/cm² | 12 – 20 Sek. | White powder | |||||
ROWALIT® BIOPOW 1038 | Biobased Products, Copolyester | 85 – 85 °C DSC | 5 g / 10 Min. (MFI 190°C) | ✓ | ✓ | ✓ | ✓ | ✓ | 40 °C | 63 °C | 125 – 150 °C | 3 – 5 N/cm² | 12 – 20 Sek. | White powder | |||||
ROWALIT® 400-1 | Copolyester | 118 – 123 °C DSC | 30 g / 10 Min. (MFI 160°C) |
0 – 63 µm 0 – 80 µm |
80 – 160 µm 80 – 200 µm | 0 – 160 µm | 100 – 500 µm | ✓ | good | no | no | 80 °C | yes | 100 °C | 130 – 150 °C | 3 – 5 N/cm² | 10 – 12 Sek. | White powder | |
ROWALIT® 400-2 | Copolyester | 110 – 115 °C DSC | 15 g / 10 Min. (MFI 160°C) | 0 – 80 µm | 80 – 200 µm | ✕ | ✓ | ✓ | good | no | no | 60 °C | fair | 95 °C | 130 – 150 °C | 3 – 10 N/cm² | 12 – 20 Sek. | White powder | |
ROWALIT® 400-8 | Copolyester | 118 – 125 °C DSC | 35 g / 10 Min. (MFI 160°C) | 0 – 80 µm | ✓ | ✕ | ✓ | ✕ | fair | no | no | 60 °C | fair | 100 °C | 125 – 145 °C | 3 – 5 N/cm² | 12 – 20 Sek. | White powder | |
ROWALIT® 400-14 | Copolyester | 177 – 186 °C DSC | 110 g / 10 Min. (MFI 190°C) | 0 – 80 µm | ✓ | ✕ | ✓ | ✓ | good | no | 90 °C | yes | 140 °C | 210 – 230 °C | 3 – 10 N/cm² | 12 – 20 Sek. | White powder | ||
ROWALIT® 400-SIT-18 | Copolyester | 110 – 120 °C DSC | 30 g / 10 Min. (MFI 160°C) | 0 – 80 µm | 80 – 200 µm | ✓ | ✓ | ✓ | good | no | 60 °C | good | 80 °C | 110 – 135 °C | 3 – 5 N/cm² | 10 – 20 Sek. | White powder | ||
ROWALIT® 400-20 | Copolyester | 70 – 85 °C DSC | 150 g / 10 Min. (MFI 160°C) | ✓ | ✓ | ✓ | ✓ | ✓ | low | yes | 40 °C | low | no | 70 °C | 90 – 120 °C | 2 – 4 N/cm² | 10 – 15 Sek. | White powder | |
ROWALIT® 400-21 | Biobased Products, Copolyester | 60 – 75 °C DSC | 35 g / 10 Min. (MFI 190°C) | 0 – 80 µm |
80 – 160 µm 80 – 200 µm | 0 – 200 µm | 100 – 500 µm | ✓ | yes | 30 °C | 75 – 95 °C | 3 – 5 N/cm² | 10 – 25 Sek. | White powder | |||||
ROWALIT® 400-29 | Biobased Products, Copolyester | 110 – 120 °C DSC | 34 g / 10 Min. (MFI 160°C) | 0 – 80 µm | 80 – 200 µm | ✕ | ✓ | ✓ | good | no | no | 60 °C | no | 100 °C | 120 – 140 °C | 3 – 5 N/cm² | 10 – 12 Sek. | White Powder | |
ROWALIT® 400-37M | Copolyester | 110 – 120 °C DSC | 20 g / 10 Min. (MFI 160°C) |
0 – 63 µm 0 – 80 µm | 80 – 200 µm | ✓ | ✓ | ✓ | good | no | no | 60 °C | 100 °C | 115 – 140 °C | 3 – 5 N/cm² | 10 – 20 Sek. | |||
ROWALIT® 400-40 | Copolyester | 105 – 120 °C DSC | 40 g / 10 Min. (MFI 160°C) | 0 – 80 µm | 80 – 200 µm | ✓ | ✓ | ✓ | 60 °C | 100 °C | 115 – 130 °C | 3 – 5 N/cm² | 10 – 20 Sek. | ||||||
ROWALIT® 400-41 | Biobased Products, Copolyester | 110 – 120 °C DSC | 20 g / 10 Min. (MFI 160°C) | 0 – 80 µm | 80 – 200 µm | ✓ | ✓ | ✓ | moderate | no | no | 40 °C | yes | no | 100 °C | 125 – 150 °C | 3 – 5 N/cm² | 12 – 20 Sek. | White powder |
ROWALIT® BIOPOW 4042 | Biobased Products, Copolyester | 65 – 75 °C DSC | 55 g / 10 Min. (MFI 160°C) | 0 – 80 µm | 80 – 200 µm | ✓ | ✓ | ✓ | moderate | yes | no | 40 °C | 55 °C | 80 – 110 °C | 3 – 5 N/cm² | 12 – 20 Sek. | White powder | ||
ROWALIT® 400-44 | Biobased Products, Copolyester | 110 – 120 °C DSC | 45 g / 10 Min. (MFI 160°C) |
0 – 63 µm 0 – 80 µm | 80 – 200 µm | ✓ | 100 – 500 µm | ✓ | good | no | 60 °C | good | 100 °C | 115 – 130 °C | 3 – 5 N/cm² | 10 – 20 Sek. | White powder |